Fig. 5. (A) Scanning electron microscope (SEM) photo of unannealed iron. (B) Surface of unannealed iron after treating an aqueous solution containing solid-phase HMX. (C) Surface of unannealed iron following treatment of an aqueoussolid-phase HMX mixture with 2% (v/v) didecyl.